Objectives: To evaluate the effects of different solutions, surface treatments, and repair materials on the shear bond strength (SBS) between aged 3D-printed provisional materials and repair materials. Methods: This study printed samples with 3D-printed resin and divided them into 16 groups (n=10): non-immersion and three solutions (40% ethanol, heptane, and cola) × two surface treatments (no abrasion [NA] and sandpaper and sandblasting [SP&SB]) × two repair materials (Poly(methyl methacrylate) [PMMA] and bis-acryl). The samples were immersed in the solutions for six days and then surface-treated. Nine samples were randomly selected for surface examination, including surface roughness, surface characteristics, and contact angle. Then, they were bonded with the repair materials, followed by 2,500 cycles of thermocycling. SBS was determined using a universal testing machine, and failure modes were determined by stereomicroscope. A three-way ANOVA was conducted to evaluate the effects of the solution, surface treatment, and repair material on SBS. SBS, surface roughness, and contact angle were compared among groups using one-way ANOVA, followed by post-hoc Tukey’s tests. Results
📖 افتح في inklap 🔗 DOI 📮 اطلب بحثاً